16-09-2006, 10:58 AM
gday , 3 hours since laying glass how long should i leave it before applying flocoat,non waxed resin.


nicko

Chimo
16-09-2006, 01:00 PM
Hi Nicko

If it was waxed resin within 24 hrs to avoid sanding. As it wasnt and if you used approx 1 % mekp it should go off pretty quickly.

So flocoate probably as soon as you can

Good luck, what you making?

Cheers

Chimo

Edencraft
16-09-2006, 08:27 PM
I hope you don't catalyse your polyester resin at 1% as you will never achieve proper cure due to low exotherm, even more important at this time of year with cooler conditions. Polyester resin is ussually catalyzed at between 1.5 and 3% depending on temp/humidity and working time required. Rather than backing of your catalyst you are better of going an LA catalyst if working time is your main concern. You can flowcoat as soon as the laminate has gone off however if it has been more than 24 hours you will have to sand the surface to get a good mechanical bond.

nicko233
24-09-2006, 08:54 AM
nothing special chimo just tydying up my anchor well lid.